Quick answer: Custom Branding for Industrial Cases starts with the process: 12–20 μm screen ink, 8–15 μm pad ink, 3 mm minimum letters, ±1 mm registration.

Table of contents

  • Four marking processes: cost against life
  • Screen ink thickness and abrasion cycles
  • Moulded letters: cut once, never peel
  • Minimum letter height and colour registration
  • Artwork handover: vector, colour reference, position drawing
  • FAQ

1. Four marking processes: cost against life

The same logo can differ threefold in life between a flat panel and a grained one. The first question in Custom Branding for Industrial Cases is which process the panel accepts, not which artwork looks best. Screen printing lands ink flattest on a plane; pad printing transfers it to curves and narrow edges; an in-mould label embeds printed film; moulded letters grow out of the steel.

Costs differ in structure: screen and pad spend on frames and fixtures, so unit cost falls with volume; in-mould labels spend on film and a pick-and-place arm, priced by a 0.3 mm sheet; moulded letters cost most once, at tooling. Life tracks the ink-to-panel bond.

ProcessFilm thicknessAbrasion cyclesMinimum letter height
Screen printing12–20 μm5003 mm
Pad printing8–15 μm500, thinner film shows through first3 mm
In-mould label0.3 mmLasts with the shell3 mm
Moulded lettersSame body as the wallNo ink, only the crown wears3 mm

Decide by panel, then volume, then change frequency. A flat ABS panel takes screen printing; a grained PP panel sheds ink, so choose pad printing with a primer or a polished patch left in the tool. Low volume with frequent changes beats a tool change, and in Custom Branding for Industrial Cases a decade-old artwork is where moulded letters amortise.

2. Screen ink thickness and abrasion cycles

Custom branding for industrial cases in use: closed black case on a wooden floor, blank front panel facing the camera, guitars and an amplifier behind.
Custom branding for industrial cases in use: closed black case on a wooden floor, blank front panel facing the camera, guitars and an amplifier behind.

Film thickness is the number most easily left vague in screen work. Custom Branding for Industrial Cases treats 12–20 μm as the normal band, built from mesh count, squeegee angle and the number of passes, never from thinning the ink. Too thin and the pigment cannot cover the shell colour, so a light print over a dark case turns grey. Too thick and the surface skins over while the layer below shrinks; the edges lift first and wear resistance drops.

How the 500-cycle test is run matters more than the figure. A loaded head rubs across the mark and the lettering must still read in full at the end. Test the thinnest stroke, where the film is shallowest; test the middle of a solid block and every process passes, which proves nothing.

Grain adds another variable: the same 12–20 μm laid over a texture sits on thousands of peaks, so contact area is half that of a flat panel and wear falls with it. Where grain is unavoidable, Custom Branding for Industrial Cases asks for a small flat patch moulded into the panel and prints there.

3. Moulded letters: cut once, never peel

The letters are part of the shell, so wearing through one layer leaves another. The cost hides in the tool: height, stroke width and draft freeze before the steel is cut, and changing a letter later means changing a mould. Custom Branding for Industrial Cases reserves moulded letters for model plates and factory marks that hold a decade, leaving dealer details to screen printing.

Taller is not better. Letters standing far above the panel get scraped by the cavity wall on ejection and pull white; letters sunk too low vanish under the grain. The compromise keeps the crown under half a millimetre proud, with fillets at the root so the letter releases on draft.

Moulded letters wear too, in a different way. Ink is rubbed away; a moulded letter is rubbed flat, the crown rounding first while the stroke shallows. Years of stiff brushing leave the edges blunt and the word legible, which is why outdoor equipment prefers it to ink.

4. Minimum letter height and colour registration

Custom branding for industrial cases, pre-press stage: blue racks holding screen-printing frames and templates, each screen stored by pattern number before transfer.
Custom branding for industrial cases, pre-press stage: blue racks holding screen-printing frames and templates, each screen stored by pattern number before transfer.

A 3 mm letter height is the floor shared by all four routes, because below it stroke width approaches the flow limit of the ink. Chinese crossbars suffer more than Latin verticals: at 3 mm a thin serif stroke breaks into dots while a gothic face holds. Custom Branding for Industrial Cases marks the minimum size on the position drawing at layout stage, before artwork is finished and found unprintable.

Two-colour work needs registration allowance on top. Keep drift between the two screens within ±1 mm and the eye reads it as aligned; exceed it and dark type over a light ground shows a white edge, while light type over dark smears into a blob. In Custom Branding for Industrial Cases, half that stability lives in how frames are numbered: the racks hold each screen under its own pattern number, and both screens share one set of stops.

A branding panel of 80×40 mm is the easiest place to overfill: type pushed to the border runs off at the first shift, while a margin lets the shift disappear. The ±1 mm figure is a gauge for acceptance, not a design target.

5. Artwork handover: vector, colour reference, position drawing

Nine logos in ten arrive as a screenshot and blur when enlarged. The first handover rule in Custom Branding for Industrial Cases is vector: closed curves, no gradients, type outlined, AI or EPS. Bitmaps print only after accepting soft edges or paying for a redraw.

Colour is specified separately, not pointed at on a screen: emitted light and reflected ink diverge, so the same orange looks warm on a monitor and prints red on a shell. State the colour reference and the order of the two colours, since whichever lies down first sets the overlap tone.

Handover itemFormatMust stateCommon mistake
Logo vectorAI or EPSOutlined, no gradientBitmap only, soft edges enlarged
Colour referenceColour number plus physical chipOverprint order of the two coloursScreen pick only, prints off-tone
Position drawingPDF with dimension lines80×40 mm panel and centre linesNo centre line, ±1 mm unjudgeable
Sample approval sheetSigned PDFFilm thickness, abrasion, adhesionAppearance signed, thickness ignored

Five days for a sample is normal, and three things need confirming: where the film lands in the 12–20 μm band, whether ink travels with the 3M 610 tape, and whether the thinnest stroke joins up. Leave one vague and rework follows.

Marking verdict: if more than 5% of the ink lifts after a 3M 610 tape peel, or the lettering loses strokes after 500 abrasion cycles, the process is rejected for that panel.