Quick answer: Precision Components Transport Case holds ±0.02 mm by aligning the datum, keeping foam compression at 10%–15% and placing six to nine support points.
Table of contents
- Part tolerance against the case datum
- How foam compression eats the margin
- Flatness and the number of support points
- Dimensional drift from temperature and humidity
- The ruling when the case is opened
- FAQ
A precision part earns its tolerance on the machine tool and then loses it in the case, and the loss rarely comes from vibration. It comes from foam compression. Part deviation, datum offset, the millimetres foam squeezes away and the stretch a temperature swing adds together make the number read after the lid opens. A Precision Components Transport Case narrows that chain one link at a time.
1. Part tolerance against the case datum
A drawing says ±0.02 mm, and that figure belongs to the part measured against its own datum face. By the time it leaves the machine most of the budget is spent. Inside a case the datum becomes whatever faces the mould produced, and once the two disagree, part of the 0.02 mm is spent by the shell instead of the part.
Shrinkage deepens the gap: ABS runs 0.4%–0.7% and PP 1.0%–2.5%, and even after the cavity is scaled up, long and short sides do not shrink alike.
A Precision Components Transport Case takes its datum from the flat base moulded in one shot, never across the parting line and never from the lid insert. The cut-out keeps 1–2 mm clearance per side, so flanks locate the part on light contacts. Clamp it and the operator tugs it free, the datum shifts, and the first point is out.
| Datum choice | Where the error enters | Result at three points |
|---|---|---|
| Flat base moulded in one shot | Same direction as the part datum | Readings cluster, usable for a ruling |
| Face taken across the parting line | Mould half offset stacked in | One long side reads positive along its length |
| Lid insert used as datum | Two mouldings plus foam rebound | Readings fail to repeat after each open |
With this link tight, the chain moves to the gap between cavity and part, which foam fills.
2. How foam compression eats the margin
Softer foam is not safer foam. At 10%–15% compression the pad still works in its rebound range and absorbs small road shocks without passing them to the wall. Past 20% it enters the densified range, reserve nearly disappears, and shock crosses into the part. This step takes the largest share of tolerance, which is why a Precision Components Transport Case gives a band rather than a figure.
Compression set of ≤5%, measured at 25% deflection for 24 h at 23 ℃, is the floor a pad must hold. It decides whether the case still seats a part after a season in a warehouse. Once set passes that limit the cavity has grown shallower, the part no longer meets the same support face, and the re-measurement drifts for reasons nobody can see.
| Compression band | State after closing | Share of the tolerance taken |
|---|---|---|
| Under 8% | Pad still free, no preload | Part roams, half the budget gone |
| 10%–15% | Rebound and support balanced | Within three tenths of the budget |
| Above 20% | Densified range reached | Shock passes through, reserve spent |
The figure is cavity depth minus part height, divided by free foam thickness, and only a result inside 10%–15% goes to sampling. Denser sheet compresses less within the 25–45 kg/m³ EVA range; mix two densities in one Precision Components Transport Case and the pads no longer squeeze alike.
3. Flatness and the number of support points
Flatness of 0.05 mm describes the support face, not the part. An uneven face lifts one corner first, and 0.05 mm over a 300 mm length becomes a reading that leans the same way everywhere, so three measurements trace one slope instead of a scatter.
Six to nine points is the working range. Three define a plane; beyond that the part shares load. At six the weight splits along two edges, and past nine the constraint grows dense enough that part and face bind. A Precision Components Transport Case places points by stiffness, denser under a flexible middle.
| Support points | Constraint state | Base layout |
|---|---|---|
| Three | One plane defined | Temporary seating for a large part |
| Six | Load split along two edges | Standard precision work |
| Nine | Constraint on the dense side | Extra points under a thin wall |
Count and flatness are read together: enough points on an uneven face load a handful of them, while a flat face with too few lets the middle sag. A Precision Components Transport Case records both on one sheet.
4. Dimensional drift from temperature and humidity
A 15 ℃ swing is ordinary across four seasons, and a case that sits in air conditioning by day and on a dock at night crosses it in hours. Linear expansion for plastics sits at 70–90×10⁻⁶/K, so a 300 mm part crossing 15 ℃ moves about 0.36 mm at 80×10⁻⁶/K, an order of magnitude above the ±0.02 mm on the drawing.
Moisture is the second path. ABS takes up 0.2%–0.45% of its weight in 24 h, and water in the shell swells the cavity wall before a dry season shrinks it back. A Precision Components Transport Case lets the pad absorb that movement.
Thicker foam does not solve drift: a thicker pad compresses further and spends the reserve before the part travels. Subtract drift from the tolerance first, then divide what remains between location and compression.
5. The ruling when the case is opened
Three points are the minimum sample, at the two far ends and the middle, measured after the case returns to about 20 ℃ so gauge and part share a temperature. Precision Components Transport Case judgement reads: if any one of the three points after opening falls outside ±0.02 mm, the foam compression band and the support point count both go back for review.
When one point is out, check compression first and points second; changing case dimensions straight away is the wrong move. Only when both check out do datum and moulding accuracy come into question on a Precision Components Transport Case.
Three items belong on the sheet: the temperature inside at opening, the three measured values, and the measured compression. With one missing, the ruling is a guess.
Conclusion
A Precision Components Transport Case holds accuracy in a fixed order: datum aligned, compression inside 10%–15%, six to nine points placed, drift removed from the budget, and only then the three-point check allowed to speak. Let one link go and the other three carry it.
This article covers only the specifications and design meaning of the container (case) itself, not any handling, loading or use of the items inside.
Related Reading
- How a high-precision sensor tray case splits its cavities
- Foam insert or divider set: which to choose
- Cavity volume and the usable ratio at the corners
- Configuring a case for calibration equipment
JUNZHIJIA
Related Products
- 8 Series — Gun Cases; Military Equipment Cases; Camera Equipment Cases; Drone Cases; Watch Cases; Knife Cases; First Aid Cases; Electronics Equipment Cases
- WL8-2812 PP Gun Case — model WL8-2812
- All protective cases and toolboxes: 7 series, 158 models